Прокладки для морских теплообменников: коррозия, материалы и запасные части.

18-11-2026

Marine Plate Heat Exchanger Gaskets: Corrosion, Materials & Spares


A seawater-cooled plate heat exchanger fails in a different order from a land unit. The plates usually outlast the gasket, and the leak that ends up in the bilge often starts in a groove rather than in a channel. Getting marine heat exchanger gaskets right means matching three things at once: plate alloy, gasket compound, and how the unit is actually run at sea.


Why Seawater Changes the Plate, Not Just the Gasket


Seawater carries roughly 19,000 mg/L of chloride. 316L is a sound choice to about 2,000 ppm and no further, so on the seawater side the plate moves up to a seawater plate heat exchanger titanium build; 254 SMO covers brackish or warmer duties. Titanium is not right everywhere: above about 80 °C, with a tight crevice, it can crevice-corrode. A gasket groove is a crevice.


Choosing a Plate Heat Exchanger Gasket for Seawater


The gasket sees the same water but answers to a different set of things. EPDM is the default for the seawater and central cooling side, and for hot water and glycol circuits. NBR and HNBR take fuel, lube oil and oily bilge duty, FKM where fuel meets higher temperature. Seawater alone rarely kills an EPDM gasket. Heat ageing, compression set and the cleaning regime do.


Where Marine Heat Exchanger Corrosion Starts


Two places matter more than the plate pack. The first is under the gasket: deposits settle in the groove, chloride concentrates, and pitting begins beneath a gasket that still looks sound. The second is the port and distribution area, where velocity drops and shellfish larvae settle. Chlorination controls fouling, but overdosing damages the wrong materials and leaves deposits that hide the next problem.


Heat Exchanger Spare Parts for Ships


Carry one gasket set per critical unit, and a spare plate set where the duty is seawater. Gaskets have a shelf life of two years, and should stay clear of sunlight, ozone and engine-room heat. Keep the set that came out: an old gasket identifies the plate pattern faster than any drawing. After a rebuild, record the A-measurement, because the next crew will need it.


What to Send for a Quote


Tag photo, plate photo, plate count, medium and temperature, and the cleaning chemicals in use. No class society issues a certificate for a gasket, but if the unit sits in a classed system, agree any material substitution with the surveyor before fitting it.


Send the duty and a photo of the tag to info@newroc-phe.com.

Получить последнюю цену? Мы ответим как можно скорее (в течение 12 часов)

Политика конфиденциальности